Test material number | Test material | Preparation steps | Binder |
---|---|---|---|
# 1 | Stone wool fibers without binder | Heat treatment at 590 °C for 20 min; sieving to < 63 μm | Removed by heat treatment |
# 2 | Milled stone wool fibers without binder | Heat treatment at 590 °C for 20 min; milling | Removed by heat treatment |
# 3 | Milled stone wool fibers sample with binder | Milling | PUF (3.5% (w/w)) |